The laminating problem of paper and nonwovens

Author: Date2014-5-11 9:56:49 Visits:

 When hot melt coating & laminating machine is used to laminate the paper and nonwovens, a problem will always happen. When the hot melt glue is coated on the paper and laminated with nonwovens, the paper will be longer and longer than the nonwovens along with machine running. The reason of this phenomenon should be two below: 
1.The problem should be caused by tension of nonwovens. The tension of nonwovens is not controlled well, and makes the nonwovens shorten after laminating.
 2.The rewinding shaft is not big enough. Because the material will lost elasticity after laminating, the material outside will be longer than the one inside.
 

Previous:没有了!
Next:PUR Hot Melt Adhesive is a special hot melt adhesive
Print || Close
Copyright © 2014 Ruian Xuteng Machinery Co.,Ltd
E-mail:xutengjx@vip.163.com
Tel:86-577-65153258 / 65153278  Fax:86-577-65153268
Add:388 Hongyuan Road, Economic Development Zone, Ruian City, Zhejiang Province. China
技术支持
点击这里给我发消息
技术支持
点击这里给我发消息